Below is the assay report of 4 different sites.
This test was done by a company on the east coast. Haber, inc.
The company recommends that I evaluate 60 lbs of each material. However,
they are on the east coast.
Extraction and recovery results. Micro Wave Digest with Aqua Regia
Using laboratory testing not using the Aladdin Methodology
Unoptimized results 100 gram samples of each ore was treated.
Sulfide Extraction Recovery
Sample Assay Tailing Recovery reduction cycle cycle Initial Au
Sample AU oz/ton AU oz/ton % Au extracted Hours Hours Hours purity
% Formulation
1 3.067 0.150 95% 0.35 1.2 0.25 98 Process hp7 modified
2 3.947 0.200 95% 0.3 1.1 0.25 99 Process hp7 modified
3 36.433 1.450 96% 0.45 1.3 0.4 98 Process hp9 modified
4 2.507 0.100 96% 0.3 1.2 0.3 98.5 Process hp7 modified
Would like some advice on further in the assessment of these materials.
And secondly, locating a facility where I could run 2 tons/hr or a similar
production rate.
The mines are near Ridgecrest, California.
Thank you,
Paul 310-279-9944
This test was done by a company on the east coast. Haber, inc.
The company recommends that I evaluate 60 lbs of each material. However,
they are on the east coast.
Extraction and recovery results. Micro Wave Digest with Aqua Regia
Using laboratory testing not using the Aladdin Methodology
Unoptimized results 100 gram samples of each ore was treated.
Sulfide Extraction Recovery
Sample Assay Tailing Recovery reduction cycle cycle Initial Au
Sample AU oz/ton AU oz/ton % Au extracted Hours Hours Hours purity
% Formulation
1 3.067 0.150 95% 0.35 1.2 0.25 98 Process hp7 modified
2 3.947 0.200 95% 0.3 1.1 0.25 99 Process hp7 modified
3 36.433 1.450 96% 0.45 1.3 0.4 98 Process hp9 modified
4 2.507 0.100 96% 0.3 1.2 0.3 98.5 Process hp7 modified
Would like some advice on further in the assessment of these materials.
And secondly, locating a facility where I could run 2 tons/hr or a similar
production rate.
The mines are near Ridgecrest, California.
Thank you,
Paul 310-279-9944