This numbers are pretty close.
Learn to do your math first before starting your process:
It takes about 38 ml of nitric acid to dissolve 1 troy oz. of silver.
It takes 48ml of nitric to dissolve Sterling Silver
It takes about 129.2 ml of nitric acid to dissolve 1 troy ounce of copper.