How much 60% nitric per Oz of sterling silver.I cheched the site and saw no math on this.Just a simple answer would be great.
 
Rule of thumb 30% nitric (what you have cut in half with distilled water- add acid to water never water to acid) 2 gallons per 100 ounces of sterling silver

So 76 ml per ounce of sterling or 38 ml of distilled water and 38 ml of 60% nitric per ounce.
 