No, the phosphoric acid will interfere with many reactions, rendering it useless.
To use it, you would have to carefully distill out the nitric acid. This will work quite well if done in reduced pressure giving clear, quality nitric. Do not overheat the residuals, as phosphoric acid will etch glass when it is concentrated and hot.
Lou