If you are speaking about the BGA Chips, then you should seek out Patnor. He has a very informative PDF on how to process those. He sells a copy on EBay for a few bucks. I have purchased it, and it was well worth the few dollars.

Steven
 
http://xtreview.com/images/nForce-680i-LT-SLI-650-SLI/northbridge-nForce-680i-LT-SLI.jpg

this is a "flip-chip" and is considered to be worthless as far as PM content.i incinerated and digested a five pound sample and wasnt able to reclaim any amount of gold.
 
Geo said:
http://xtreview.com/images/nForce-680i-LT-SLI-650-SLI/northbridge-nForce-680i-LT-SLI.jpg

this is a "flip-chip" and is considered to be worthless as far as PM content.i incinerated and digested a five pound sample and wasnt able to reclaim any amount of gold.


Geo anything in the green fiber board part?? tim
 
i incinerated the whole green board. i then milled them and removed as much fiberglass as i could. i processed the entire mass in AR in two separate batches and neither tested positive for gold. the "flip-chip" processors are a waste of time and chemicals.
 
I usually use a blow torch on a low heat setting. I really want to try the hot sand method I saw on youtube!
 