Found some interesting things as I was digging into some of my long forgotten stuff. These are from a circuit board of an old calculator. Most of the discrete components had gold plating on the ends, both inside and out. Tested a few in AP and the foils came off intack, nice thick plating. Just thought I'd pass this along incase anyone else has some old stuff, a quick scratch will tell. (I swear, someday I'm going to actually see the floor in my garage again.)