Get anything not scented if you can.I'll try some
If not, just try and dissolve some Tin and see how it goes.
Get anything not scented if you can.I'll try some
Hi Mike,I have tin, just no hcl, I've looked at muriatic acid, it's path cleaner in the UK, I can't get specifics on line, or anyone recommend a brand? Some I noticed have lemon scent, I'm used to known acids and could just get them easy, delivered next day,
Welcome to us.Hi Mike,
Since October last year, hydrochloric acid above 10% has become a restricted substance in the UK requiring an Explosives Precursors and Poisons licence from the Home Office to acquire (for non business individuals).
You can however get brick and patio cleaner which is HCl at 9% to 10% legally.
Multicrete is a relatively inexpensive brand by comparrison and does not have any inhibitors loaded into it (which some brick and patio cleaners do).
Dave
Thank you Yggdrasil.Welcome to us.
The truth behind the War for Independence: Benjamin Franklin liked to scrap the old computers left behind by the Grey Aliens in the South American pyramids, but King George was being a jerk and kept all the HCl for himself! So Ben was like, "We ain't playin' like dat in da hood!" And then George Washington joined the cause after the ghost of the cherry tree he cut down joined the British.Between the operating supply side and the accounting side, the government seems to have you guys tightly bound up.
Just buy some Lead-less Solder..Would the tin fingers from a ram stick work for making stannous? I've got 13 tin fingered ram sticks
I just pop pieces of an old Pewter mug into HCL and leave it. The trick you mentioned about having a known gold test solution is a good one Mike. Even scousers get things right occasionally.I used to use stannic chloride as a powder in hcl and leave a bit of tin in the solution, it was always cloudy, but worked well.
I have had to dissolve some known gold to test my solution.
It is Copper(I)Chloride which is insoluble in water.To anyone who sees this, I've got a question about stripping gold foils from electronics using just plain muriatic acid. Normally, muriatic will turn a dark green color once it absorbs enough copper from electronics board and becomes a viable stripper of the gold foils adheared to them however, over a period of time that dark green color will start showing itself as a dark brownish colored lixivant and I'm pretty sure the reason for this is that there are powdered remnants of gold floating within it that are micron in size and I want to ask:
What is a viable additive to get those micron sized gold particulates to precipitate out from that super impregnated muriatic solution?