This gold came from a deplating cell that I posted about here:
http://www.goldrefiningforum.com/phpBB3/viewtopic.php?f=40&t=27077&p=287181#p287181
From material I posted about here:
http://www.goldrefiningforum.com/phpBB3/viewtopic.php?f=34&t=5023&p=287182#p287182
The gold was Dissolved Twice in AR.
The AR looked right, good color.
I tried to use minimal SMB to avoid any drag down. A little less then a 1:1 ratio.
After dropping the solution was nice and clear both times.
The powder was a nice light brown color.
But, I got a strange "stain" on the button when it was melted.
Can anyone tell me what this "stain" is?
My scale weighs it at 31.280 grams
http://www.goldrefiningforum.com/phpBB3/viewtopic.php?f=40&t=27077&p=287181#p287181
From material I posted about here:
http://www.goldrefiningforum.com/phpBB3/viewtopic.php?f=34&t=5023&p=287182#p287182
The gold was Dissolved Twice in AR.
The AR looked right, good color.
I tried to use minimal SMB to avoid any drag down. A little less then a 1:1 ratio.
After dropping the solution was nice and clear both times.
The powder was a nice light brown color.
But, I got a strange "stain" on the button when it was melted.
Can anyone tell me what this "stain" is?
My scale weighs it at 31.280 grams