Our first leaching of button sample

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

plasmasmelter

Well-known member
Joined
Aug 31, 2010
Messages
63
One small step in the longer process of getting to a refineable
product we can get paid for. :lol: Diluted battery acid from junk
battery. Will be crushing samples with new ball mill we are
making and scale up this operation. We also took a sample
and crushed it and crudely separated the magnet attracting
particles from the non-magnet attracting particles and leaching
them separately just to see what happens while we are building
a small production milling and leaching system.
 

Attachments

  • DSC00901.JPG
    DSC00901.JPG
    3.5 MB
Are you using the Ball Mill as the first step? Are you milling black sand? Do you still soak it? If so, before or after the mill?