Our Gold Recovery & Refining Project -- Begging for... "Assay"

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
You are right to be concerned about concentrated sulfuric acid. Avoid at all costs, especially when heated. Yes, it dissolves plastic, but also dissolves skin, clothing, and anything organic. A single drop can cause serious damage.

As for removing lead from your gold foils solution, dilute sulfuric acid is perfectly fine, even preferred. The amount of lead present is typically small, and instantly precipitates out as lead sulphate. Stay safe, and avoiding concentrated H2SO4 is a good start whenever possible.
 