Can some one tell me a simple best way to process these kind of gold tape and wires from different electronics mixed together ? Please !?
 

Attachments

  • 20210207_120346_HDR.jpg
    20210207_120346_HDR.jpg
    3.9 MB · Views: 116
  • 20210207_120540_HDR.jpg
    20210207_120540_HDR.jpg
    3.4 MB · Views: 116
  • 20210207_120706_HDR.jpg
    20210207_120706_HDR.jpg
    3.7 MB · Views: 116
Heres more pics
 

Attachments

  • 20210207_120454_HDR.jpg
    20210207_120454_HDR.jpg
    3.6 MB · Views: 113
  • 20201122_112122_HDR.jpg
    20201122_112122_HDR.jpg
    4 MB · Views: 113
  • 20201021_041916.jpg
    20201021_041916.jpg
    5.4 MB · Views: 113
Not a lot of gold on those pieces. Not enough to warrant special treatment and running it in a separate batch.

I deal with them in two ways. First I trim off anything not gold using a pair of scissors. I throw the non-gold parts in with my low grade boards and sell it.

Then, if I have a copper chloride leach running I just toss the gold plated parts in there. The underlying copper dissolves and the gold mixes with the gold from the fingers I'm running.

Otherwise if it's just a few pieces I just toss it in with my old filters that I will incinerate. The same thing here, the little gold there is will mix with the rest and I'll recover it all when I process old filters.

Göran
 
g_axelsson said:
Otherwise if it's just a few pieces I just toss it in with my old filters that I will incinerate. The same thing here, the little gold there is will mix with the rest and I'll recover it all when I process old filters.

Göran

That' s what I do with them :mrgreen:

Edit to add; - after cutting the gold only part off the ribbons

Kurt
 