Hi all..
Went to my Rona.. and all they have is Muriatic Acid HCl 20degre /Be
will it do the work ? and should i change something to my receipe ? wich is :
150g of pins
8oz Nitrate Soda for 480ml hot water (can i take taped water)
960ml HCl + (Nitrate + H2O)
Since my HCl is only 20... should i put a litle more.. or keep the receip like this ( i saw some one who was reducing is HCl (32%) by 50% and was working well but slower.. as i am not in a rush.. what you suggest ?