Poor man's pyrolysis

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Joko sulistyo

Well-known member
Joined
Nov 2, 2015
Messages
48
Hi,all.
I will share about simple and cheap pyrolysis.This is what I do when burning IC chip or cellphone boards.You only need a used paint can.Make two hole on the lid.Put IC chip in the can and close the lid.Burn the can into fire/furnace for 20 minutes.With this way,IC will burned into carbon without any smell.After done,transfer the carbonized IC into another can and burn once again without lid.The result is IC will be ash completely.How your opinion?
 

Attachments

  • IMG_20210226_150306_compress47.jpg
    IMG_20210226_150306_compress47.jpg
    565 KB · Views: 219
  • IMG_20210226_143400_compress21.jpg
    IMG_20210226_143400_compress21.jpg
    575.9 KB · Views: 219
  • IMG_20210226_142433_compress63.jpg
    IMG_20210226_142433_compress63.jpg
    545.5 KB · Views: 218
  • IMG_20210226_140838_compress24.jpg
    IMG_20210226_140838_compress24.jpg
    533.7 KB · Views: 216
kjavanb123 said:
Hmm

You sure about no smoke? Fumes that come out need to be burned with air.

I don't know about with IC chips (haven't tried this with them), but this is the method I use to make charcoal. While making charcoal, flames burn out of the holes until flammables are consumed.
 