I did not fix the garbage disposal today clean up the garage somewhat . But had an itch to make some buttons .
20.4 gram
3.4 gram
Not happy with the surface glaze from the flux but I haven’t put it in the pickle jar .
Yes sir I did knock it down some
I heated from the bottom for a good bit
I was afraid the gold would blow out it’s my third time handling gold powder .
I use a turbo torch