Pouring First Bar; Concerns

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Anslow

Member
Joined
Feb 1, 2022
Messages
12
Location
Washington State
Hey y’all, long time reader first time poster.
I just purified my first ounce of gold, had it XRF’ed and it was .99 fine. Very happy with the results.
Since I just melted a large button I haven’t put it into a mold yet. Its a little splotchy and not clean so I want to remelt it into a mold. My issue is that I have this wild fear that the gold will pop when I pour it into the mold. I’ve read about sooting, preheating for moisture, and about using a flame for the pour. Will this guarantee no loss due to gold popping out or is there anything else I can do to prevent this? Thanks a lot for your time; sorry if this is a repeat post, the search was 39 pages and after about 10 I just decided to post. Cheers!
 

Attachments

  • 3FFC8214-0454-4D35-A6E4-9F7EF75766A8.jpeg
    3FFC8214-0454-4D35-A6E4-9F7EF75766A8.jpeg
    2.4 MB · Views: 13
  • 999448B6-6FFC-490C-9918-AD3D5F1DA6A5.jpeg
    999448B6-6FFC-490C-9918-AD3D5F1DA6A5.jpeg
    2 MB · Views: 13
Back
Top