• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

powder containing 25%Silver and 75%Tin

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
i have a powder containing 25% of silver and 75% of tin--how can i separate the Silver from the tin? thanks for any help.
The Tin will dissolve in HCl Silver will not.
And at this concentration the Tin should completely dissolve I believe.
 
Not sure if using HCl will create silver chloride especially in powder form but I think caustic soda will dissolve tin especially if heated , should you choose that option be very careful caustic is nasty and even worse if hot.
Try a couple of small samples using both methods and pick the one that suits your needs.
 
i have a powder containing 25% of silver and 75% of tin--how can i separate the Silver from the tin? thanks for any help.

We need more information about this powder

Such as -----------

How fine is the powder - powder could be considered anything from 40 mesh in size to 300 mesh & even finer

It can make a difference on how chems will react with it --- example - at 40 mesh HCl would likely dissolve the tin leaving the silver with little or no effect on the silver - but at 300 mesh the HCl "may" create some AgCl

Is the powder an alloy of tin/silver - or is it tin powder - mixed - with silver powder

Kurt
 
We need more information about this powder

Such as -----------

How fine is the powder - powder could be considered anything from 40 mesh in size to 300 mesh & even finer

It can make a difference on how chems will react with it --- example - at 40 mesh HCl would likely dissolve the tin leaving the silver with little or no effect on the silver - but at 300 mesh the HCl "may" create some AgCl

Is the powder an alloy of tin/silver - or is it tin powder - mixed - with silver powder

Kurt
This seems to be essentially silver 'inquarted' with tin. Should that be enough to dissolve the tin in HCl even if it's an alloy?
 
I think the silver will be covered with a chloride crust and will partially seal some of the tin if you use hydrochloric acid, besides, it (the chlorine crust) will not be dissolved by nitric acid...
I think direct dissolution in nitric acid and cementation on copper is more practical.
 
I think the silver will be covered with a chloride crust and will partially seal some of the tin if you use hydrochloric acid, besides, it (the chlorine crust) will not be dissolved by nitric acid...
I think direct dissolution in nitric acid and cementation on copper is more practical.

I’m not sure mixing nitric and tin would be my choice of process for this material…trying to filter the solution full of metastatic acid would be a nightmare .
 
I’m not sure mixing nitric and tin would be my choice of process for this material…trying to filter the solution full of metastatic acid would be a nightmare .
Exactly what I thought too.
Maybe the Sodium Hydroxide route is better, but I have never tried that.
 
I’m not sure mixing nitric and tin would be my choice of process for this material…trying to filter the solution full of metastatic acid would be a nightmare .
time...
gravity...
decantation...

and no filtration
 
It's been a while, but there is a process by which you add lead chloride to molten tin/lead solder that is contaminated with gold. The lead chloride makes slag that will carry a considerably higher percentage of gold. It was posted on this forum before. I want to say it was GSP who posted it, but I can't remember for sure...and I have no clue if it would work. But, it's easy enough to test.
 
It's been a while, but there is a process by which you add lead chloride to molten tin/lead solder that is contaminated with gold. The lead chloride makes slag that will carry a considerably higher percentage of gold. It was posted on this forum before. I want to say it was GSP who posted it, but I can't remember for sure...and I have no clue if it would work. But, it's easy enough to test.
I think it is the parkes process.
It can be used to extract Gold or Silver from Lead.
If you melt it and add Zinc or Aluminum the Silver/Gold has a higher Solubility in Zn/Al than Lead and it forms a slag like compsition that can be skimmed or filtered off.
Not sure if it works with Tin though.
 
i have a powder containing 25% of silver and 75% of tin--how can i separate the Silver from the tin? thanks for any help.
How "sharp" do you need the separation to be ?

If you know about Parkes process (pulling silver from molten lead with zinc), same can be done also with tin based alloy. However, the extraction of silver from molten tin is not that efficient as with lead based alloys.

I have personally done it, but with 3% Ag in tin, and it kinda worked, I think I managed to get below 0.6(+-)% of Ag in leftover tin. Advantage is that tin has lower melting point than lead and this can be conveniently done in stainless steel pot insulated with some glass/mineral wool, using heatgun as heating source applied from below. This allow for precise temperature control.

I do not know how the such high Ag alloy react to this treatment, as melting point would be risen due to Ag content.

If you can get the alloy for a good price, then this may be a relatively easy route, and in the end you will have reasonable silver fraction ready to be refined + you will sell the "skimmed" tin with some minor silver in it (essentially alloy like non-leaded solder).

--------
We also tried electrolytic enrichment of silver by electrolysis in molten tin chloride, but this is very messy and very unplesant. It kinda works, but I will stick to the zinc skimming if I would to process this for first try. Then maybe some hydrometallurgy...
 
How "sharp" do you need the separation to be ?

If you know about Parkes process (pulling silver from molten lead with zinc), same can be done also with tin based alloy. However, the extraction of silver from molten tin is not that efficient as with lead based alloys.

I have personally done it, but with 3% Ag in tin, and it kinda worked, I think I managed to get below 0.6(+-)% of Ag in leftover tin. Advantage is that tin has lower melting point than lead and this can be conveniently done in stainless steel pot insulated with some glass/mineral wool, using heatgun as heating source applied from below. This allow for precise temperature control.

I do not know how the such high Ag alloy react to this treatment, as melting point would be risen due to Ag content.

If you can get the alloy for a good price, then this may be a relatively easy route, and in the end you will have reasonable silver fraction ready to be refined + you will sell the "skimmed" tin with some minor silver in it (essentially alloy like non-leaded solder).

--------
We also tried electrolytic enrichment of silver by electrolysis in molten tin chloride, but this is very messy and very unplesant. It kinda works, but I will stick to the zinc skimming if I would to process this for first try. Then maybe some hydrometallurgy...
You do not need to skim it.
If one builds a stainless filter tube with fiberglass filter cloth it can be vacuum or pressure filtered.
There was an interesting article where they tested Zinc Vs Aluminum as collector.
Zinc was best for Ag and Au did best with Al.

This was done in Lead though.

Hmm.
A combination of Owltechs Gold/Lead solution and the Parkes process could be interesting.
 
You do not need to skim it.
If one builds a stainless filter tube with fiberglass filter cloth it can be vacuum or pressure filtered.
There was an interesting article where they tested Zinc Vs Aluminum as collector.
Zinc was best for Ag and Au did best with Al.

This was done in Lead though.

Hmm.
A combination of Owltechs Gold/Lead solution and the Parkes process could be interesting.
We filtered it, but you need to pay very good attention to the filter construction and heat it uniformly, to a precise temperature :D any makeshift attempts to just filter it with some heatgun in hand resulted in catastrophic solidification across all of the filter :D

Then, we mostly used "aging" of the precipitate by slow cooling and coalescing of the grains of formed Ag3Zn alloy. This was then possible to strain through very tight stainless screen.
 
Well, I know most people fear to use it... but sulfuric acid is a possibility here. With tin, it doesn't need to be concentrated. Normally, tin in diluted sulfuric acid reacts slowly. But with powder, it'll react much more quickly.

Silver should not react much, if at all with dilute sulfuric, as far as I can find out. However, if it does form some silver sulfate, that's still insoluble. So no matter what, the tin will be gone and you'll be left with solids that are only silver. There are several methods for turning silver sulfate back to silver.
 
I have to agree with Anarxi, direct dissolution in nitric acid will work as long as the nitric acid is dilute and kept cold. the formation of metastannic acid will be minimized shifting the reaction to the production of tin nitrate instead. then cementation of the silver on copper leaving the tin in solution. the production of metastannic acid is highly integrated with the concentration of nitric acid and time of exposure. in other words , if you choose this route do not let your solutions stand around. would also be prudent to test on small amounts.
 