Haha i like that^


I will be good to get some more brains in this venture..


My setup is like this atm:

Running 24 V   7 A power. I tryed 24v and 10A, but could'n se any differince.

My glas bowl is around 4 litres/~1,5gal i think.

Catode/anode is sitting aprox 5inc from itchothers- i tryed mohing both closer and longer distance, but could not see any chance.

I have now cleanet the silver of 1 spoon, and 2 suger cups at the size of a grown mans fist, and i think all in all it has run for 12-15h. It won't get the silver inside thise cups, so i'm saveing them, and then i will flatten out with a hammer. I should allso mention that i'm turning the cups as they get strippet, course it seems that they only get strippet on the side facing the catode-or maybe i just needs more patien and it will get there:)

I now have a bit more than 0,5inch gryish sediment on the botten, and the botten of my bowl is messuring 6-7inch in diameter.


Hope this all makes sense.