silversaddle1 said:
bee said:
i have processed tons of ram. the Au yield is always arround .8gram per 1000 grams of ram and i donot cut fingers we grind and melt the dust with PbO + flux.
thanks
bee

So then what is your average yield per pound for Ram?

My math is not very good anymore but I was guessing about 2.5 pounds of Ram will net about 1 gram of gold. Sound about right?

Well according to the math, using his yield number, it would be 2.75 lbs of ram per 1 gram of gold. (using 454 grams per pound).
 