I have a solution which is a mix of Silver nitrate, Zinc and Gold. Is there any method of recovering the gold from such a solution?

Looking forward to replies. Thank you
 
What is the form of zinc? Zinc chloride?
What is the form of gold? Gold chloride?
What is the pH of the solution?

Have you tried cementing with copper? This will drop everything below its reactivity series.
 
Is there any gold worth recovering, if it's only a nitric solution you shouldn't have gold in solution, is this the pour off from inquarting? If so simple filtering should remove any gold particles.
 