Recovering tin copper from auto connecters.

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

tiggertree

Member
Joined
Feb 9, 2022
Messages
15
Location
North Wales
I have few thousand copper or brass tin plated new auto connectors.
Some have gold plate on the connecting areas.
I intend to recover the tin and copper first.
I read a while back a paper that used a solution of sulphuric acid and copper sulfate to dissolve the metals. Then to use 2v and 3v constant voltage supply to recover the tin and copper separately to a carbon anode.
I cannot now find the paper.?.
As any one here any advice on setting this up?
Cheers.
Paul. From Wales uk.
 
Back