It is pretty heavy gauge yea is is punching scrapsgoldsilverpro said:Is that stuff in the photo made from real thin stock? It's hard to tell. I have seen heavy gauge, gold filled brass punchings scrap, that looks the same.
O no no not that thick! Not like a badgegoldsilverpro said:I shouldn't get you excited. It's probably exactly what Steve says it is. He has some of it and recognizes it to be the same stuff. The stuff I saw was at least 1/16" (1.6 mm) and was used to stamp out police badges.
It is 0.67mm and 0.026ingoldsilverpro said:I shouldn't get you excited. It's probably exactly what Steve says it is. He has some of it and recognizes it to be the same stuff. The stuff I saw was at least 1/16" (1.6 mm) and was used to stamp out some kind of round badges.
goldsilverpro said:Is that nickel at the upper left?
I would put 100% of my energies into getting all of the gold and staying safe. The amount of impurities makes little difference, as far as the purification process goes.