cupellation problems :
has anyone had this problem before? i guess platinum family is messin with me.
 

Attachments

  • IMG_20240830_225652282_PORTRAIT.jpg
    IMG_20240830_225652282_PORTRAIT.jpg
    1.3 MB
  • IMG_20240831_161722346_PORTRAIT.jpg
    IMG_20240831_161722346_PORTRAIT.jpg
    4.9 MB
  • IMG_20240831_161504351_HDR (3).jpg
    IMG_20240831_161504351_HDR (3).jpg
    2.1 MB
Welcome to us.
Platinum metals pose no problem in cupels.
What do you have in the cupel?
Describe in detail please.
i have a prill from smelting ore with flux's at about 1250 . i belive i half assed scorification with only 2 to 1 lead and cupelled at about 860
 
i have a prill from smelting ore with flux's at about 1250 . i belive i half assed scorification with only 2 to 1 lead and cupelled at about 860
removing the value, its brittle and theres a rose color powder and gold flakes. some cupells come out with red arms. amazon test stuff says 22k or better, also platinum. so im not getting solid metal.
 