The least you can do, is get your Chemicals right. It is Aqua Regia and Pd will also dissolve in Nitric.So basically if you're trying to refine palladium and then cement that PD with copper foils or bars. that the best way to do it is to use a concentrated version of aquaria will dissolve the palladium and then you'll precipitation with SMB or formic acid.