I would recommend a set of thick chemical golves and eye/face protection. Don't get any oxalic acid or it's salts in your mouth.

Steve
 
after reading noxx"s tutorial on the butyl diglyme i have a question. in the tutorial he disolved all ready some what refined gold. how would this process work on "dirty" AR? IE from ceramic cpu's or boards?

Or should this process be reserved for "final clean up"

Ryan
 
BDG will also be able to extract gold from «dirty» AR solution. Just be sure to follow the patent...

I think the link is broken. Let me fix this.
 
The tutorial have been reposted in thread http://goldrefiningforum.com/phpBB3/viewtopic.php?f=37&t=10883&p=227729#p227729

Göran
 
Art, I'm guessing you clicked on the link in Noxx's original post that Göran quoted. It's probably because GRF is no longer hosted by 110MB.COM. They probably default any unfound pages to the advertising. If you click on the link Göran provided below the quoted material, you'll see the original material Noxx wrote.

Dave
 