Hi all. Let’s get right to the point. I thought I’d try and extract all the gold from my old filters by adding them to the foils for the hcl/ bleach process. All went well, solution went yellow and filtered into a flask. But I’m left with a yellow mash in the filter that won’t let go of the aucl (positive stannous test). Anyone got any hot tips of getting the gold out?