Now i am having a hard time finding out Returns on Gold pins from electronics Like Computers
I have run some myself but i like to check returns other are receiving to see if my iodine leaching method is working well or not.
I like to Know what more modern Computer pins should return
per pound how many grams or fractions of a gram thanks of 90-99% gold
should i be recovering on the low end and on the high end thanks
Joshua
I have run some myself but i like to check returns other are receiving to see if my iodine leaching method is working well or not.
I like to Know what more modern Computer pins should return
per pound how many grams or fractions of a gram thanks of 90-99% gold
should i be recovering on the low end and on the high end thanks
Joshua