simulacra10
New member
- Joined
- Mar 23, 2011
- Messages
- 3
I'm studying like crazy and I think the most efficient method seems to be reverse electroplating. After watching some of the videos and reading posts I have a few questions.
1. After electroplating I understand that the precious metal is then deposited on the bottom in the form of sludge. Is it the sludge that I then need to take and further refine?
2. When watching one of the videos, Steve's I think, he add glycerin to the sulfuric acid, is that actually necessary as that seems to be the only place that I have seen that mentioned as an ingredient.
3. Thanks to all who keep this forum alive and to the Mods for the awesome handbook provided.
Norm
1. After electroplating I understand that the precious metal is then deposited on the bottom in the form of sludge. Is it the sludge that I then need to take and further refine?
2. When watching one of the videos, Steve's I think, he add glycerin to the sulfuric acid, is that actually necessary as that seems to be the only place that I have seen that mentioned as an ingredient.
3. Thanks to all who keep this forum alive and to the Mods for the awesome handbook provided.
Norm