A simple way to reduce your rinse water without loosing any potential values.
cut a 3"x3" pipe, attach a screen to the top using a hose clamp,stuff it full of fiberglass insulation
Using a ss pressure cooker without a valve put the filter on the pressure cooker and reduce your rinse water.
Just leave the reduced liquid in the pot.when you have reduced what you think is enough to recover the values,process the filter and the water with a little ar.
just pondering
john
P.S. Would you like to hear my ponder for making a gas or electric classifier?
cut a 3"x3" pipe, attach a screen to the top using a hose clamp,stuff it full of fiberglass insulation
Using a ss pressure cooker without a valve put the filter on the pressure cooker and reduce your rinse water.
Just leave the reduced liquid in the pot.when you have reduced what you think is enough to recover the values,process the filter and the water with a little ar.
just pondering
john
P.S. Would you like to hear my ponder for making a gas or electric classifier?