samuel-a

Well-known member
Joined
Oct 7, 2009
Messages
2,190
Make sure you don't toss them with the rest of your low grade stuff, those are heavy plated little jewels...

I found mine in an old Decade boxes, a few dozen of them...
DSC01690.JPG
DSC01693.JPG
DSC01702.JPG

According to the maker, this specific type are 3 um plated gold, that's sound resnoble knowing what their tasks are...

I had this little piece (in pic 3 on the left) soaking in nitric, and was left with intact gold foils with the same original shape, this is a good indicator for thickness... plus, a tiny bit of silver came out of there...
The other pins are still soaking in AP.


Have a good urban mining
 
are they cars?

Edit, Oh boy,
I wanted to type are they from cars, like used to control the fan or heater.

jim
 
http://www.keison.co.uk/cropico_rbb_decadebox.shtml
Probably something similar to this.
 