A ashir Well-known member Joined Aug 17, 2018 Messages 256 Nov 27, 2020 #1 Hi every one. I need 200 mesh size of ore. After tha ball mill i want seive the material . Looking for ideas to construct a seiver, already have a shaker type seiver but the powder not flow on seive and make a hole in seive. Any aidea?
Hi every one. I need 200 mesh size of ore. After tha ball mill i want seive the material . Looking for ideas to construct a seiver, already have a shaker type seiver but the powder not flow on seive and make a hole in seive. Any aidea?
Shark Well-known member Joined Jun 8, 2014 Messages 3,005 Location Alabama Dec 3, 2020 #2 How much material do you wish to run at one time?
A ashir Well-known member Joined Aug 17, 2018 Messages 256 Dec 3, 2020 #3 Shark said: How much material do you wish to run at one time? Click to expand... if you ask for material per day then its 500 kg per day. I have this type of shaker to seive material. 2 diffrent mesh size seiver can be added at a time material is feed with controable cone. Matarial not run properly and some time make holes in mesh
Shark said: How much material do you wish to run at one time? Click to expand... if you ask for material per day then its 500 kg per day. I have this type of shaker to seive material. 2 diffrent mesh size seiver can be added at a time material is feed with controable cone. Matarial not run properly and some time make holes in mesh