This is a short tutorial demonstrating the separation of silver and gold using Nitric Acid. The initial weight of silver/gold mix weighed 41.5 grams.
Here is the initial silver gold mix used:
Please post your comments and suggestions as usual.
I've provided this video as a standalone playlist located at my website. You must click the "I Agree" link and you will see the video lists. Select the "Separating Silver from Gold" link to open the videos for this tutorial.