Hey,
I now came to my first stock pot refining. I have a solution wich is not seethrough and greenish/blackish (Most of it is CuCl2 and NiCl2). There should be some silver in it because 3 months ago I put all my wastes together in one bucket and Silver Chloride appeared when pouring it in. Now its just a greenish black liquid without any white AgCl in solution. Now I did put some of the solution into a beaker and added HCl but no Silver Chloride appeared. Does someone know where my silver could have gone?
David
Edit: I just use AP (HCl, H2O2) Solutions with Sodiumhypochloride and SMB (No nitric, No sulfuric, ...)
I now came to my first stock pot refining. I have a solution wich is not seethrough and greenish/blackish (Most of it is CuCl2 and NiCl2). There should be some silver in it because 3 months ago I put all my wastes together in one bucket and Silver Chloride appeared when pouring it in. Now its just a greenish black liquid without any white AgCl in solution. Now I did put some of the solution into a beaker and added HCl but no Silver Chloride appeared. Does someone know where my silver could have gone?
David
Edit: I just use AP (HCl, H2O2) Solutions with Sodiumhypochloride and SMB (No nitric, No sulfuric, ...)
Last edited: