Hi,
I am going insane! I am trying to pour silver into a Durston combination bar form 4.5mm x 50mm x 80mm. It was a scrap silver therefore I am not sure if I mixed 999 with 925 - does it matter when melting? So I bring the silver in my crucible to a nice liquid form, I heat the mold and when I pour into the mould it does not come out as a nice solid, even and regular bar. It looks like silver expanding foam in a mini version. What do I do wrong? I tried 5 times with no success so far. :evil:
I am going insane! I am trying to pour silver into a Durston combination bar form 4.5mm x 50mm x 80mm. It was a scrap silver therefore I am not sure if I mixed 999 with 925 - does it matter when melting? So I bring the silver in my crucible to a nice liquid form, I heat the mold and when I pour into the mould it does not come out as a nice solid, even and regular bar. It looks like silver expanding foam in a mini version. What do I do wrong? I tried 5 times with no success so far. :evil: