H h hutch1945 Member Joined Apr 29, 2013 Messages 11 May 5, 2013 #1 anyone of you had any experience refining these silver mylar sheets, from computer keyboards, thanks
Claudie Well-known member Joined Aug 17, 2010 Messages 1,853 Location Iowa May 5, 2013 #2 Actually yes, there is a lot of information about them on the forum. Search for "keyboard mylars". There are a couple of active threads about them right now. EDIT: http://goldrefiningforum.com/phpBB3/search.php?keywords=keyboard+mylars&terms=all&author=&sv=0&sc=1&sf=all&sk=t&sd=d&sr=posts&st=0&ch=300&t=0&submit=Search
Actually yes, there is a lot of information about them on the forum. Search for "keyboard mylars". There are a couple of active threads about them right now. EDIT: http://goldrefiningforum.com/phpBB3/search.php?keywords=keyboard+mylars&terms=all&author=&sv=0&sc=1&sf=all&sk=t&sd=d&sr=posts&st=0&ch=300&t=0&submit=Search
solar_plasma Well-known member Joined Feb 27, 2013 Messages 2,695 Location Germany May 6, 2013 #3 As far as you are familar with using acids, this is the only process, which is really as easy as it looks like.
As far as you are familar with using acids, this is the only process, which is really as easy as it looks like.