So in the image below we are parting the inquarted gold with nitric acid, we are able to achieve close to three nines fine gold which is good enough for us.
Parting with nitric requires multiple nitric boils and we wish to siphon the boiling nitric using a pump, we would like to collect any siphoned gold in an overflow tank and process it later.
We have attached a glass rod to the teflon pipe which will be submerged in the acid at all time and used for siphoning when needed.
We are in an ideation phase and looking for ideas to improve the design.
The key challanges we have at this point.
1. What should be the material used for siphoning(is the teflon pipe good enough and will last a long time(or what other materials can be used, is a peristaltic pump good for this use case(if so what consideration needs to be taken while choosing a pump), how to join the teflon tube and the glass pipe in the beaker).
2. Is there a way to isolate the inquarted gold during siphoning to minimise the gold in the overflow tank?
I have read through the forum and found people are using teflon pipes and teflon valves to connect the reaction vessel to a Condensor, I am guessing my piping and motor will be exposed to the same harsh conditions, my main concern is the longevity of the apparatus and a safe working environment.
Thanks.
Regards.
Amol
Parting with nitric requires multiple nitric boils and we wish to siphon the boiling nitric using a pump, we would like to collect any siphoned gold in an overflow tank and process it later.
We have attached a glass rod to the teflon pipe which will be submerged in the acid at all time and used for siphoning when needed.
We are in an ideation phase and looking for ideas to improve the design.
The key challanges we have at this point.
1. What should be the material used for siphoning(is the teflon pipe good enough and will last a long time(or what other materials can be used, is a peristaltic pump good for this use case(if so what consideration needs to be taken while choosing a pump), how to join the teflon tube and the glass pipe in the beaker).
2. Is there a way to isolate the inquarted gold during siphoning to minimise the gold in the overflow tank?
I have read through the forum and found people are using teflon pipes and teflon valves to connect the reaction vessel to a Condensor, I am guessing my piping and motor will be exposed to the same harsh conditions, my main concern is the longevity of the apparatus and a safe working environment.
Thanks.
Regards.
Amol