S sourdoughjoe Member Joined Nov 8, 2007 Messages 16 Location Savannah, MO Nov 15, 2011 #1 What is the correct ratio of SMB to gold weight to use in AR solution to peripitae gold out of solution? Thanks...Joe!
What is the correct ratio of SMB to gold weight to use in AR solution to peripitae gold out of solution? Thanks...Joe!
jimmydolittle Well-known member Joined Sep 15, 2011 Messages 157 Location Southern Indiana Nov 15, 2011 #2 Use equal parts of SMB to the amonut of gold you estimate to be in solution, plus a little extra, just in case. Test the solution after the gold has dropped out with stannous chloride.
Use equal parts of SMB to the amonut of gold you estimate to be in solution, plus a little extra, just in case. Test the solution after the gold has dropped out with stannous chloride.
S sourdoughjoe Member Joined Nov 8, 2007 Messages 16 Location Savannah, MO Nov 15, 2011 #3 Thanks for the info...Joe!