I've found to get a good pour into a mold, without it setting too quick before it takes the shape of the mold, get it to that "white hot" stage. It should take a good 5 seconds before it sets AFTER having been poured into the mold. Helps to heat your mold as well, as has been posted bunches of times in various places around the forums.