After a long waiting, I video recorded our smelting process.
Feed materials are actually components depopulated manually from about 74 lbs of mixed motherboards and 2 kg of cards.
They were pyrolized prior to smelt. Please leave comments.
I will be doing more sample smelting specially on cell phone boards, ceramic catalytic converters and telecomm boards.
You can check out the video at
https://youtu.be/Ttv-qLxTs90
Best regards
Kj