A arthur kierski Well-known member Joined Feb 10, 2008 Messages 1,090 Location são paulo---brazil Mar 28, 2009 #1 please tell me how many mls of nitric acid(70%) corresponds to x grams of sodium nitrate----------------example:100grams of nano3= xmls of hno3(70%) thanks for the reply
please tell me how many mls of nitric acid(70%) corresponds to x grams of sodium nitrate----------------example:100grams of nano3= xmls of hno3(70%) thanks for the reply
lazersteve Well-known member Joined Feb 27, 2007 Messages 7,334 Location Florida Mar 28, 2009 #2 Arthur, I've answered this in detail here: Nitric to Sodium Nitrate The short answer is ~1.34 grams of NaNO3 per mL of 70% HNO3 Steve
Arthur, I've answered this in detail here: Nitric to Sodium Nitrate The short answer is ~1.34 grams of NaNO3 per mL of 70% HNO3 Steve
A arthur kierski Well-known member Joined Feb 10, 2008 Messages 1,090 Location são paulo---brazil Mar 28, 2009 #3 thanks again great STEVE for your imediate reply