D dogger brian Member Joined Aug 30, 2008 Messages 12 Location winchester uk Dec 26, 2008 #1 hi has anyone processed solar cells for pm i have 10kg of this lot.. all i know that the wire is copper plated with silver are there other pgms worth recovering thanks brian
hi has anyone processed solar cells for pm i have 10kg of this lot.. all i know that the wire is copper plated with silver are there other pgms worth recovering thanks brian
SilverFox Well-known member Joined Aug 4, 2008 Messages 143 Location Ohio Dec 26, 2008 #2 Dissolve some in some HCL Clorox, then do a stannous chloride tests. (Tin and HCL) 30 ml HCL to 1 gram tin then post pictures of the color swab, I like using qtips for this..
Dissolve some in some HCL Clorox, then do a stannous chloride tests. (Tin and HCL) 30 ml HCL to 1 gram tin then post pictures of the color swab, I like using qtips for this..