Started working on a sample my son brought home from a prospecting trip to Nevada. Sample was off a big boulder trip through the jaw crusher - Chain mill - panned - swept with a magnet no magnetics. What I thought was black sands is purple? sand this ore is really hard and new to us but just tried a small piece I see Gold.
 

Attachments

  • 20241207_124759.jpg
    20241207_124759.jpg
    1.2 MB
  • 20241207_130210.jpg
    20241207_130210.jpg
    255.3 KB
  • 20241207_125328.jpg
    20241207_125328.jpg
    1.3 MB
  • 20241207_125733.jpg
    20241207_125733.jpg
    278.7 KB
  • 20241207_132049.jpg
    20241207_132049.jpg
    468 KB
  • 20241207_131955.jpg
    20241207_131955.jpg
    474 KB
  • 20241207_132002.jpg
    20241207_132002.jpg
    396.4 KB
Started working on a sample my son brought home from a prospecting trip to Nevada. Sample was off a big boulder trip through the jaw crusher - Chain mill - panned - swept with a magnet no magnetics. What I thought was black sands is purple? sand this ore is really hard and new to us but just tried a small piece I see Gold.
The color makes me think of a pan with a lot of small garnets. (Dan Hurd)
 
No.
Iridescence is changing colors due to viewpoint/reflection like butterfly wings and such and Fluorescence is emitting colored light in response to electromagnetic radiation like UV light.
You're right, I based my reaction on the iridescent mineral in the picture Southfork shared, with an oily surface shine. I have not read properly.
 
"looks like purple fluorite' or "galena" - so, a simple test that distinguishes between them and a fun/useful tool in the bag of tricks searchig for and identification of minerals.
 
"looks like purple fluorite' or "galena" - so, a simple test that distinguishes between them and a fun/useful tool in the bag of tricks searchig for and identification of minerals.
Southfork first posted a picture showing crushed and panned material. It is hard to discern what it was at that point, as it could only be described as purple. Upon posting a clear picture of the mineral crystal, it was very clearly Galena. Easier to know your minerals than carry a bunch of testing equipment into the field.
 
Apart from Probably Galena
is impressive the amount of others Sulphide
in that pan
Very Impressive for that small test.
send an example to a lab ,perhaps You will get a very good news

Northwestern Nevada is Known to have telluride with up to 30-40 % gold in it
and lot of silver.
 
Apart from Probably Galena
is impressive the amount of others Sulphide
in that pan
Very Impressive for that small test.
send an example to a lab ,perhaps You will get a very good news

Northwestern Nevada is Known to have telluride with up to 30-40 % gold in it
and lot of silver.
I still have a couple of pounds to mill and pan to extract the free gold if there is any. And maybe a smelt or just melt some powdered rock then have a look. Nevada is a great place to prospect I'm just trying to get caught up on samples from Northern California and Nevada.
 