Just would like to share with you something I didn't know but first ive been scrapping out the newer tv's and there's a small strip board running across the top that just pops out has a surprising amount of gold on them. Also was trimming fingers on some finger cards when I noticed some scratches so I started scraping the solder mask away and the entire card is plated in gold the ones I noticed where called sound blaster boards and are all solid black but since I've found quite a few others. I sell the boards after I trim the gold fingers off and I can honestly tell y'all I have sold hundreds of these boards. Just something to lookout for for those who don't know. Just trying to help keep