M6MR&R
Member
- Joined
- Jan 12, 2015
- Messages
- 10
i used to get beautiful large Crystals growing all over the bowl but for some reason i now get soft fluffy redddish brown fiber looking stuff. I have taken the fluffy crystals and rinsed dried and melted them and they look very beautiful. My problem is i can only run the cell for a few hours before i have to remove these reddish brown crystals. When it dries it looks like cemeted silver from copper plate.
Im using approximate 475g of Au in 4L of electrolyte. 1.8amp @3.1v .
Im using approximate 475g of Au in 4L of electrolyte. 1.8amp @3.1v .