Not for melting silver or gold. You can stretch cast iron to melt silver in, and maybe gold, but not stainless. Generally speaking, you don't melt metals in other metals because they like to dissolve each other, and braze themselves together.
Melting precious metals in metallic vessels of any kind would be a huge mistake. Both gold and silver are more than eager to solder to other elements, and each are solvents of other metals. The moment you allow molten metals to contact other metals, you contaminate them.