Hi guys,
So I put 10g of tin shots into 50mL of 31.45% HCl in order to make stanous chloride, but it's been well over 48 hours and the tin shots look like they haven't dissolved at all. I even tried putting the mixture over a candle to heat it up, but I got no results. But the mixture is still bubbling.
I even separated the time shots from the HCl and sighed the tin shots to see if anything was dissolved and they still weighed 10g.
Any suggestions how to properly make stanous with tin shots and HCl? I don't have any stanous crystals.