Hello,
I'm currently working through my box of ceramic CPUs and thought it would be helpful to post up my results. I ran them through AR twice then used my kiln and oxy-acetylene touch to cast it. I did the same with the fingers but after leaving them in AP for around a week.
I'm putting together a list for me so that I have a ballpark figure of what the yield is. Here are my results so far:
101.7g x foils from various fingers - 58.25g
89 x Ceramic AMD Athalon - 4.3g
70 x AMD K6 - 2.6g
79 x intel pentium ceramic - 5.31g
16 x Intel Pentium w/mmx - .39g
Will have results for the following next week:
- Will be a few weeks until I can do another batch, but will keep updating
I'll keep on updating this post with what I get and what's coming up next. I'm getting all of my lower yielding ones out of the way first, and moving onto the better ones later.
I'm currently working through my box of ceramic CPUs and thought it would be helpful to post up my results. I ran them through AR twice then used my kiln and oxy-acetylene touch to cast it. I did the same with the fingers but after leaving them in AP for around a week.
I'm putting together a list for me so that I have a ballpark figure of what the yield is. Here are my results so far:
101.7g x foils from various fingers - 58.25g
89 x Ceramic AMD Athalon - 4.3g
70 x AMD K6 - 2.6g
79 x intel pentium ceramic - 5.31g
16 x Intel Pentium w/mmx - .39g
Will have results for the following next week:
- Will be a few weeks until I can do another batch, but will keep updating
I'll keep on updating this post with what I get and what's coming up next. I'm getting all of my lower yielding ones out of the way first, and moving onto the better ones later.