Strange colour borax

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Ferrit69

Member
Joined
Sep 18, 2011
Messages
8
Location
County Durham, England
DSC_0011_crop_181x179.JPG
I melted a small quantity of electrical contacts today and the borax went blue. Has anyone seen this before and what metal has caused it?
I stopped at that point until I find out what it is.
 
Never melt electrical parts unless you know what's in them.

Looks like molybdenum blue.

Probably lots of white smoke?
 
I melt in good extracted area I thought of cobalt as it looks that colour, no white smoke when melted. Cadmium has not been used in contacts in England for a very long time the switches they came out of are only 1 year old.
 
Lino1406 said:
At temperature close to MPs of cobalt or Molybden borax should evaporate

As pure metals maybe but what's the effect of melting them with another lower melting point metal?
 
Lino1406 said:
At temperature close to MPs of cobalt or Molybden borax should evaporate
It’s not that they melt. The oxides become soluble in the borax.


Sent from my iPhone using Tapatalk
 