L Lino1406 Well-known member Joined Nov 1, 2007 Messages 2,356 Location Israel Apr 13, 2017 #21 I meant, if aluminum is confirmed, you can also use HCl to consume it not necessarily NaOH, to avoid rinsing. Then decant and proceed to normal procedure - meaning A/P to consume copper and nickel
I meant, if aluminum is confirmed, you can also use HCl to consume it not necessarily NaOH, to avoid rinsing. Then decant and proceed to normal procedure - meaning A/P to consume copper and nickel
K kurtak Well-known member Joined Jan 16, 2014 Messages 4,012 Location John Day Oregon Apr 14, 2017 #22 Though this type connecters are often made of aluminum - they can also be die cast which is primarily zinc To confirm aluminum - or - zinc - test with nitric Both aluminum & zinc will react with HCl Aluminum does "not" react with nitric - but - does react with zinc Kurt
Though this type connecters are often made of aluminum - they can also be die cast which is primarily zinc To confirm aluminum - or - zinc - test with nitric Both aluminum & zinc will react with HCl Aluminum does "not" react with nitric - but - does react with zinc Kurt
donald7755 Well-known member Joined Mar 23, 2017 Messages 61 Apr 15, 2017 #23 anachronism said: It doesn't need to be hot it depends on how much of a rush you are in. Hot lye isn't a good substance. Click to expand... will the lye strip the gold off and then i refine as normal ?
anachronism said: It doesn't need to be hot it depends on how much of a rush you are in. Hot lye isn't a good substance. Click to expand... will the lye strip the gold off and then i refine as normal ?