Slochteren
Well-known member
I have made me a new cell and changed the setup a bit, added my airbubler to it wich is located under the basket (1 cm between hose-end and basket)to get the material a bit moving and i thought it would cool the cell also. The negative is 2 cm above the basket/material.
Since in the normal setup there were always some unfinished pins in it and i had to move the material a few times to deplate everything, now i can start the process without attention.
Added a picture of the result after my first run, looks like it worked fine as thought. Only the cooling is not as much as i expected.
Since in the normal setup there were always some unfinished pins in it and i had to move the material a few times to deplate everything, now i can start the process without attention.
Added a picture of the result after my first run, looks like it worked fine as thought. Only the cooling is not as much as i expected.
![cell.jpg](https://proxy.imagearchive.com/103/1033b20c428decd9d2fb28330bc5ecd5.jpg)
![result.jpg](https://proxy.imagearchive.com/f4c/f4c8c79e61f07ad8b2f1fff24a13962b.jpg)