Hi, these pinless CPU connectors are called Fuzz Button connectors and yes as Glondor said their yield is very high , base metal can be Beryllium copper or Molybdenum, look for Custom Interconnect Fuzz Button Connectors and Cinch's Cin::Apse website for more information. I refined a batch of 350 grams (whole connectors,75-80 gms pins approximately ) got about 28 gram fines.
I get lots of servers and the spacers with the fuzz wires are the best yielding things I ever did. There are a lot of variations and types of those fuzz wires over the years. Some have more connections than others,but the larger sparc IV processor fuzzes gave me the best yields. .65 grams of contacts (each one) yielded .4 grams of gold. The last one I did had 16 processors in it. that gave over 6 grams just for the fuzz connectors.